Cement Clinker
Guaranteed high-alite (C3S 58–66%) grey and white clinker for African cement grinding plants. Direct Supramax parcel shipments from Turkey, Egypt, and UAE with certified SGS assays.

"Uniform mineralogical granulometry (0–25mm) with certified high early-strength reactivity."

"Selective mining and bench sampling ensure strict mineralogical consistency from origin."
Homogeneous Raw Meal Stoichiometry
Our partnered kilns source from high-calcium, low-alkali limestone quarries with continuous XRF automated sampling. Sintering at 1,450°C in modern rotary pre-calciner kilns guarantees rapid hydraulic strength gain upon finish grinding.
Supply Grades
Standard Grey Portland Clinker (Type I/II)
High-grade alite clinker optimized for multi-purpose cement grinding with high clinker factor or slag/pozzolana blending.
High-Early-Strength Clinker (Type III Equivalent)
Ultra-reactive clinker with C3S > 64% and rapid 2-day compressive strength gain for fast-setting industrial binders.
White Portland Cement Clinker
Ultra-low ferric oxide clinker with high whiteness index (>88% Hunter) for architectural concrete, terrazzo, and dry-mix mortars.
Guaranteed Assay Parameters
| Parameter | Guaranteed Range | Test Method | Significance |
|---|---|---|---|
| Tricalcium Silicate (C3S / Alite) | 55.0% – 66.0% | Bogue Calculation / XRD | Dictates 28-day hydraulic compressive strength and early strength development. |
| Dicalcium Silicate (C2S / Belite) | 12.0% – 20.0% | Bogue Calculation / XRD | Governs late-stage strength development (after 28 days) and hydration heat. |
| Tricalcium Aluminate (C3A) | 7.0% – 11.0% (Grey) / <4.5% (Sulfate Resistant) | Bogue Calculation | Controls initial setting time and chemical resistance against sulfate attack. |
| Tetracalcium Aluminoferrite (C4AF) | 9.0% – 14.0% | Bogue Calculation | Fluxing agent and source of grey coloration; lower in white clinker. |
| Free Calcium Oxide (Free Lime) | < 1.50% (Typically 0.8% – 1.2%) | Ethylene Glycol Extraction | Vital for volumetric stability and sound expansion (prevents autoclave expansion). |
| Loss on Ignition (LOI) | < 0.80% (Max 1.0%) | EN 196-2 / ASTM C114 | Confirms complete calcination and minimal moisture uptake during voyage. |
| Liter Weight (Bulk Liter Density) | 1,180 – 1,350 g/L | Standard Funnel Volumetric | Key indicator of burning degree and raw meal reactivity in the kiln. |
| Total Alkali Equivalent (Na2O + 0.658 K2O) | < 0.85% | Flame Photometry / XRF | Prevents damaging alkali-silica reactivity (ASR) in concrete aggregates. |
Typical Oxide Breakdown (XRF Analysis)